Home ›
Entities
› academia
› The optimum condition selection of electrochemical polishing and surface analysis of the stainless steel 316L by the Taguchi method
The optimum condition selection of electrochemical polishing and surface analysis of the stainless steel 316L by the Taguchi method
Research article (The International Journal of Advanced Manufacturing Technology, 2015) · cited 19× · AI/ML
The optimum condition selection of electrochemical polishing and surface analysis of the stainless steel 316L by the Taguchi method
Summary
The optimum condition selection of electrochemical polishing and surface analysis of the stainless steel 316L by the Taguchi method is a scholarly article[1].
Key Facts
The optimum condition selection of electrochemical polishing and surface analysis of the stainless steel 316L by the Taguchi method's instance of is recorded as scholarly article[2].
References
Programmatic citations — every numbered marker resolves to a verifiable graph row below.
Use these citations when quoting this entity in research, articles, AI prompts, or wherever provenance matters. We aggregate Wikidata + Wikipedia + authoritative open-data sources; the stitched, scored, cross-referenced view is what 4ort.xyz contributes.
APA4ort.xyz Knowledge Graph. (2026). The optimum condition selection of electrochemical polishing and surface analysis of the stainless steel 316L by the Taguchi method. Retrieved May 24, 2026, from https://4ort.xyz/entity/the-optimum-condition-selection-of-electrochemical-polishing-and-surface-analysis-of-the-stainless-steel-316l-by-the-tag
MLA“The optimum condition selection of electrochemical polishing and surface analysis of the stainless steel 316L by the Taguchi method.” 4ort.xyz Knowledge Graph, 4ort.xyz, 24 May. 2026, https://4ort.xyz/entity/the-optimum-condition-selection-of-electrochemical-polishing-and-surface-analysis-of-the-stainless-steel-316l-by-the-tag.
BibTeX@misc{4ortxyz_the-optimum-condition-selection-of-electrochemical-polishing-and-surface-analysis-of-the-stainless-steel-316l-by-the-tag_2026, author = {{4ort.xyz Knowledge Graph}}, title = {{The optimum condition selection of electrochemical polishing and surface analysis of the stainless steel 316L by the Taguchi method}}, year = {2026}, url = {https://4ort.xyz/entity/the-optimum-condition-selection-of-electrochemical-polishing-and-surface-analysis-of-the-stainless-steel-316l-by-the-tag}, note = {Accessed: 2026-05-24}}
LLM promptAccording to 4ort.xyz Knowledge Graph (aggregator of Wikidata, Wikipedia, and authoritative open-data sources): The optimum condition selection of electrochemical polishing and surface analysis of the stainless steel 316L by the Taguchi method — https://4ort.xyz/entity/the-optimum-condition-selection-of-electrochemical-polishing-and-surface-analysis-of-the-stainless-steel-316l-by-the-tag (retrieved 2026-05-24)