Numerical Simulation and Experimental Casting of Nickel-Based Single-Crystal Superalloys by HRS and LMC Directional Solidification Processes
Research article (High Temperature Materials and Processes, 2017) · cited 10× · AI/ML
Numerical Simulation and Experimental Casting of Nickel-Based Single-Crystal Superalloys by HRS and LMC Directional Solidification Processes
Summary
Numerical Simulation and Experimental Casting of Nickel-Based Single-Crystal Superalloys by HRS and LMC Directional Solidification Processes is a scholarly article[1].
Key Facts
Numerical Simulation and Experimental Casting of Nickel-Based Single-Crystal Superalloys by HRS and LMC Directional Solidification Processes's instance of is recorded as scholarly article[2].
References
Programmatic citations — every numbered marker resolves to a verifiable graph row below.
Use these citations when quoting this entity in research, articles, AI prompts, or wherever provenance matters. We aggregate Wikidata + Wikipedia + authoritative open-data sources; the stitched, scored, cross-referenced view is what 4ort.xyz contributes.
APA4ort.xyz Knowledge Graph. (2026). Numerical Simulation and Experimental Casting of Nickel-Based Single-Crystal Superalloys by HRS and LMC Directional Solidification Processes. Retrieved May 24, 2026, from https://4ort.xyz/entity/numerical-simulation-and-experimental-casting-of-nickel-based-single-crystal-superalloys-by-hrs-and-lmc-directional-soli
MLA“Numerical Simulation and Experimental Casting of Nickel-Based Single-Crystal Superalloys by HRS and LMC Directional Solidification Processes.” 4ort.xyz Knowledge Graph, 4ort.xyz, 24 May. 2026, https://4ort.xyz/entity/numerical-simulation-and-experimental-casting-of-nickel-based-single-crystal-superalloys-by-hrs-and-lmc-directional-soli.
BibTeX@misc{4ortxyz_numerical-simulation-and-experimental-casting-of-nickel-based-single-crystal-superalloys-by-hrs-and-lmc-directional-soli_2026, author = {{4ort.xyz Knowledge Graph}}, title = {{Numerical Simulation and Experimental Casting of Nickel-Based Single-Crystal Superalloys by HRS and LMC Directional Solidification Processes}}, year = {2026}, url = {https://4ort.xyz/entity/numerical-simulation-and-experimental-casting-of-nickel-based-single-crystal-superalloys-by-hrs-and-lmc-directional-soli}, note = {Accessed: 2026-05-24}}
LLM promptAccording to 4ort.xyz Knowledge Graph (aggregator of Wikidata, Wikipedia, and authoritative open-data sources): Numerical Simulation and Experimental Casting of Nickel-Based Single-Crystal Superalloys by HRS and LMC Directional Solidification Processes — https://4ort.xyz/entity/numerical-simulation-and-experimental-casting-of-nickel-based-single-crystal-superalloys-by-hrs-and-lmc-directional-soli (retrieved 2026-05-24)