Research article (Metals, 2020) · cited 36× · AI/ML
Microstructure and Creep Properties of Ni-Base Superalloy IN718 Built up by Selective Laser Melting in a Vacuum Environment
Summary
Microstructure and Creep Properties of Ni-Base Superalloy IN718 Built up by Selective Laser Melting in a Vacuum Environment is a scholarly article[1].
Key Facts
Microstructure and Creep Properties of Ni-Base Superalloy IN718 Built up by Selective Laser Melting in a Vacuum Environment's instance of is recorded as scholarly article[2].
References
Programmatic citations — every numbered marker resolves to a verifiable graph row below.
Use these citations when quoting this entity in research, articles, AI prompts, or wherever provenance matters. We aggregate Wikidata + Wikipedia + authoritative open-data sources; the stitched, scored, cross-referenced view is what 4ort.xyz contributes.
APA4ort.xyz Knowledge Graph. (2026). Microstructure and Creep Properties of Ni-Base Superalloy IN718 Built up by Selective Laser Melting in a Vacuum Environment. Retrieved May 24, 2026, from https://4ort.xyz/entity/microstructure-and-creep-properties-of-ni-base-superalloy-in718-built-up-by-selective-laser-melting-in-a-vacuum-environm
MLA“Microstructure and Creep Properties of Ni-Base Superalloy IN718 Built up by Selective Laser Melting in a Vacuum Environment.” 4ort.xyz Knowledge Graph, 4ort.xyz, 24 May. 2026, https://4ort.xyz/entity/microstructure-and-creep-properties-of-ni-base-superalloy-in718-built-up-by-selective-laser-melting-in-a-vacuum-environm.
BibTeX@misc{4ortxyz_microstructure-and-creep-properties-of-ni-base-superalloy-in718-built-up-by-selective-laser-melting-in-a-vacuum-environm_2026, author = {{4ort.xyz Knowledge Graph}}, title = {{Microstructure and Creep Properties of Ni-Base Superalloy IN718 Built up by Selective Laser Melting in a Vacuum Environment}}, year = {2026}, url = {https://4ort.xyz/entity/microstructure-and-creep-properties-of-ni-base-superalloy-in718-built-up-by-selective-laser-melting-in-a-vacuum-environm}, note = {Accessed: 2026-05-24}}
LLM promptAccording to 4ort.xyz Knowledge Graph (aggregator of Wikidata, Wikipedia, and authoritative open-data sources): Microstructure and Creep Properties of Ni-Base Superalloy IN718 Built up by Selective Laser Melting in a Vacuum Environment — https://4ort.xyz/entity/microstructure-and-creep-properties-of-ni-base-superalloy-in718-built-up-by-selective-laser-melting-in-a-vacuum-environm (retrieved 2026-05-24)