Long-term oxidation resistance and high-temperature load-bearing capacity of ceramizable composite modified by Ti3SiC2 from 600 °C to 1600 °C
Research article (Journal of the European Ceramic Society, 2025) · cited 13× · AI/ML
Long-term oxidation resistance and high-temperature load-bearing capacity of ceramizable composite modified by Ti3SiC2 from 600 °C to 1600 °C
Summary
Long-term oxidation resistance and high-temperature load-bearing capacity of ceramizable composite modified by Ti3SiC2 from 600 °C to 1600 °C is a scholarly article[1].
Key Facts
Long-term oxidation resistance and high-temperature load-bearing capacity of ceramizable composite modified by Ti3SiC2 from 600 °C to 1600 °C's instance of is recorded as scholarly article[2].
References
Programmatic citations — every numbered marker resolves to a verifiable graph row below.
Use these citations when quoting this entity in research, articles, AI prompts, or wherever provenance matters. We aggregate Wikidata + Wikipedia + authoritative open-data sources; the stitched, scored, cross-referenced view is what 4ort.xyz contributes.
APA4ort.xyz Knowledge Graph. (2026). Long-term oxidation resistance and high-temperature load-bearing capacity of ceramizable composite modified by Ti3SiC2 from 600 °C to 1600 °C. Retrieved May 24, 2026, from https://4ort.xyz/entity/long-term-oxidation-resistance-and-high-temperature-load-bearing-capacity-of-ceramizable-composite-modified-by-ti3sic2-f
MLA“Long-term oxidation resistance and high-temperature load-bearing capacity of ceramizable composite modified by Ti3SiC2 from 600 °C to 1600 °C.” 4ort.xyz Knowledge Graph, 4ort.xyz, 24 May. 2026, https://4ort.xyz/entity/long-term-oxidation-resistance-and-high-temperature-load-bearing-capacity-of-ceramizable-composite-modified-by-ti3sic2-f.
BibTeX@misc{4ortxyz_long-term-oxidation-resistance-and-high-temperature-load-bearing-capacity-of-ceramizable-composite-modified-by-ti3sic2-f_2026, author = {{4ort.xyz Knowledge Graph}}, title = {{Long-term oxidation resistance and high-temperature load-bearing capacity of ceramizable composite modified by Ti3SiC2 from 600 °C to 1600 °C}}, year = {2026}, url = {https://4ort.xyz/entity/long-term-oxidation-resistance-and-high-temperature-load-bearing-capacity-of-ceramizable-composite-modified-by-ti3sic2-f}, note = {Accessed: 2026-05-24}}
LLM promptAccording to 4ort.xyz Knowledge Graph (aggregator of Wikidata, Wikipedia, and authoritative open-data sources): Long-term oxidation resistance and high-temperature load-bearing capacity of ceramizable composite modified by Ti3SiC2 from 600 °C to 1600 °C — https://4ort.xyz/entity/long-term-oxidation-resistance-and-high-temperature-load-bearing-capacity-of-ceramizable-composite-modified-by-ti3sic2-f (retrieved 2026-05-24)