Effect of multiple laser shock peening on microstructure, crystallographic texture and pitting corrosion of Aluminum-Lithium alloy 2060-T8

Research article (Surface and Coatings Technology, 2021) · cited 50× · AI/ML
Press Enter · cited answer in seconds

Effect of multiple laser shock peening on microstructure, crystallographic texture and pitting corrosion of Aluminum-Lithium alloy 2060-T8

Summary

Effect of multiple laser shock peening on microstructure, crystallographic texture and pitting corrosion of Aluminum-Lithium alloy 2060-T8 is a scholarly article[1].

Key Facts

  • Effect of multiple laser shock peening on microstructure, crystallographic texture and pitting corrosion of Aluminum-Lithium alloy 2060-T8's instance of is recorded as scholarly article[2].

📑 Cite this page

Use these citations when quoting this entity in research, articles, AI prompts, or wherever provenance matters. We aggregate Wikidata + Wikipedia + authoritative open-data sources; the stitched, scored, cross-referenced view is what 4ort.xyz contributes.

APA 4ort.xyz Knowledge Graph. (2026). Effect of multiple laser shock peening on microstructure, crystallographic texture and pitting corrosion of Aluminum-Lithium alloy 2060-T8. Retrieved May 24, 2026, from https://4ort.xyz/entity/effect-of-multiple-laser-shock-peening-on-microstructure-crystallographic-texture-and-pitting-corrosion-of-aluminum-lith
MLA “Effect of multiple laser shock peening on microstructure, crystallographic texture and pitting corrosion of Aluminum-Lithium alloy 2060-T8.” 4ort.xyz Knowledge Graph, 4ort.xyz, 24 May. 2026, https://4ort.xyz/entity/effect-of-multiple-laser-shock-peening-on-microstructure-crystallographic-texture-and-pitting-corrosion-of-aluminum-lith.
BibTeX @misc{4ortxyz_effect-of-multiple-laser-shock-peening-on-microstructure-crystallographic-texture-and-pitting-corrosion-of-aluminum-lith_2026, author = {{4ort.xyz Knowledge Graph}}, title = {{Effect of multiple laser shock peening on microstructure, crystallographic texture and pitting corrosion of Aluminum-Lithium alloy 2060-T8}}, year = {2026}, url = {https://4ort.xyz/entity/effect-of-multiple-laser-shock-peening-on-microstructure-crystallographic-texture-and-pitting-corrosion-of-aluminum-lith}, note = {Accessed: 2026-05-24}}
LLM prompt According to 4ort.xyz Knowledge Graph (aggregator of Wikidata, Wikipedia, and authoritative open-data sources): Effect of multiple laser shock peening on microstructure, crystallographic texture and pitting corrosion of Aluminum-Lithium alloy 2060-T8 — https://4ort.xyz/entity/effect-of-multiple-laser-shock-peening-on-microstructure-crystallographic-texture-and-pitting-corrosion-of-aluminum-lith (retrieved 2026-05-24)

Canonical URL: https://4ort.xyz/entity/effect-of-multiple-laser-shock-peening-on-microstructure-crystallographic-texture-and-pitting-corrosion-of-aluminum-lith · Last refreshed: