Effect of hot rolling temperature on microstructure evolution, deformation texture and nanoindentation properties of an intermetallic Ti-43Al-9V-0.2Y alloy

Research article (Intermetallics, 2019) · cited 16× · AI/ML
Press Enter · cited answer in seconds

Effect of hot rolling temperature on microstructure evolution, deformation texture and nanoindentation properties of an intermetallic Ti-43Al-9V-0.2Y alloy

Summary

Effect of hot rolling temperature on microstructure evolution, deformation texture and nanoindentation properties of an intermetallic Ti-43Al-9V-0.2Y alloy is a scholarly article[1].

Key Facts

  • Effect of hot rolling temperature on microstructure evolution, deformation texture and nanoindentation properties of an intermetallic Ti-43Al-9V-0.2Y alloy's instance of is recorded as scholarly article[2].

📑 Cite this page

Use these citations when quoting this entity in research, articles, AI prompts, or wherever provenance matters. We aggregate Wikidata + Wikipedia + authoritative open-data sources; the stitched, scored, cross-referenced view is what 4ort.xyz contributes.

APA 4ort.xyz Knowledge Graph. (2026). Effect of hot rolling temperature on microstructure evolution, deformation texture and nanoindentation properties of an intermetallic Ti-43Al-9V-0.2Y alloy. Retrieved May 24, 2026, from https://4ort.xyz/entity/effect-of-hot-rolling-temperature-on-microstructure-evolution-deformation-texture-and-nanoindentation-properties-of-an-i
MLA “Effect of hot rolling temperature on microstructure evolution, deformation texture and nanoindentation properties of an intermetallic Ti-43Al-9V-0.2Y alloy.” 4ort.xyz Knowledge Graph, 4ort.xyz, 24 May. 2026, https://4ort.xyz/entity/effect-of-hot-rolling-temperature-on-microstructure-evolution-deformation-texture-and-nanoindentation-properties-of-an-i.
BibTeX @misc{4ortxyz_effect-of-hot-rolling-temperature-on-microstructure-evolution-deformation-texture-and-nanoindentation-properties-of-an-i_2026, author = {{4ort.xyz Knowledge Graph}}, title = {{Effect of hot rolling temperature on microstructure evolution, deformation texture and nanoindentation properties of an intermetallic Ti-43Al-9V-0.2Y alloy}}, year = {2026}, url = {https://4ort.xyz/entity/effect-of-hot-rolling-temperature-on-microstructure-evolution-deformation-texture-and-nanoindentation-properties-of-an-i}, note = {Accessed: 2026-05-24}}
LLM prompt According to 4ort.xyz Knowledge Graph (aggregator of Wikidata, Wikipedia, and authoritative open-data sources): Effect of hot rolling temperature on microstructure evolution, deformation texture and nanoindentation properties of an intermetallic Ti-43Al-9V-0.2Y alloy — https://4ort.xyz/entity/effect-of-hot-rolling-temperature-on-microstructure-evolution-deformation-texture-and-nanoindentation-properties-of-an-i (retrieved 2026-05-24)

Canonical URL: https://4ort.xyz/entity/effect-of-hot-rolling-temperature-on-microstructure-evolution-deformation-texture-and-nanoindentation-properties-of-an-i · Last refreshed: