# Welding defects detection based on deep learning with multiple optical sensors during disk laser welding of thick plates

> Research article (Journal of Manufacturing Systems, 2019) · cited 158× · AI/ML

**Wikidata**: [openalex:W2941542910](https://www.wikidata.org/wiki/openalex:W2941542910)  
**Source**: https://4ort.xyz/entity/welding-defects-detection-based-on-deep-learning-with-multiple-optical-sensors-during-disk-laser-welding-of-thick-plates