# Testing Novel Portland Cement Formulations with Carbon Nanotubes and Intrinsic Properties Revelation: Nanoindentation Analysis with Machine Learning on Microstructure Identification

> Research article (Nanomaterials, 2020) · cited 41× · AI/ML