# Real-Time High-Performance Laser Welding Defect Detection by Combining ACGAN-Based Data Enhancement and Multi-Model Fusion

> Research article (Sensors, 2021) · cited 33× · AI/ML

**Wikidata**: [openalex:W3210242198](https://www.wikidata.org/wiki/openalex:W3210242198)  
**Source**: https://4ort.xyz/entity/real-time-high-performance-laser-welding-defect-detection-by-combining-acgan-based-data-enhancement-and-multi-model-fusi
