# Physics-informed machine learning framework for creep-fatigue life prediction of a Ni-based superalloy using ensemble learning

> Research article (Materials Today Communications, 2024) · cited 18× · AI/ML

**Wikidata**: [openalex:W4402024894](https://www.wikidata.org/wiki/openalex:W4402024894)  