# Microstructure, texture and mechanical properties of Inconel GH4169 superalloy fabricated by wire arc additive manufacturing with arc oscillation

> Research article (Journal of Alloys and Compounds, 2023) · cited 52× · AI/ML

**Wikidata**: [openalex:W4363677164](https://www.wikidata.org/wiki/openalex:W4363677164)  
**Source**: https://4ort.xyz/entity/microstructure-texture-and-mechanical-properties-of-inconel-gh4169-superalloy-fabricated-by-wire-arc-additive-manufactur