# Microstructure and Creep Properties of Ni-Base Superalloy IN718 Built up by Selective Laser Melting in a Vacuum Environment

> Research article (Metals, 2020) · cited 36× · AI/ML

**Wikidata**: [openalex:W3011541490](https://www.wikidata.org/wiki/openalex:W3011541490)  
**Source**: https://4ort.xyz/entity/microstructure-and-creep-properties-of-ni-base-superalloy-in718-built-up-by-selective-laser-melting-in-a-vacuum-environm