# Machine Learning Method for Fatigue Strength Prediction of Nickel-Based Superalloy with Various Influencing Factors

> Research article (Materials, 2022) · cited 14× · AI/ML

**Wikidata**: [openalex:W4313470115](https://www.wikidata.org/wiki/openalex:W4313470115)  
**Source**: https://4ort.xyz/entity/machine-learning-method-for-fatigue-strength-prediction-of-nickel-based-superalloy-with-various-influencing-factors