# Investigation of feed-forward back propagation ANN using voltage signals for the early prediction of the welding defect

> Research article (SN Applied Sciences, 2019) · cited 49× · AI/ML

**Wikidata**: [openalex:W2988743840](https://www.wikidata.org/wiki/openalex:W2988743840)  