# In-situ environmental TEM study of γ′-γ phase transformation induced by oxidation in a nickel-based single crystal superalloy

> Research article (Journal of Alloys and Compounds, 2015) · cited 47× · AI/ML

**Wikidata**: [openalex:W1189392439](https://www.wikidata.org/wiki/openalex:W1189392439)  
**Source**: https://4ort.xyz/entity/in-situ-environmental-tem-study-of-phase-transformation-induced-by-oxidation-in-a-nickel-based-single-crystal-superalloy