# iCHORD-SI combination as an alternative to EDS-EBSD coupling for the characterization of γ-γ′ nickel-based superalloy microstructures

> Research article (Materials Characterization, 2018) · cited 10× · AI/ML

**Wikidata**: [openalex:W2807020481](https://www.wikidata.org/wiki/openalex:W2807020481)  
**Source**: https://4ort.xyz/entity/ichord-si-combination-as-an-alternative-to-eds-ebsd-coupling-for-the-characterization-of-nickel-based-superalloy-microst