# Hierarchical microstructure and enhanced mechanical properties of SLM-fabricated GH5188 Co-superalloy

> Research article (Materials Science and Engineering A, 2021) · cited 50× · AI/ML

**Wikidata**: [openalex:W3208513144](https://www.wikidata.org/wiki/openalex:W3208513144)  
**Source**: https://4ort.xyz/entity/hierarchical-microstructure-and-enhanced-mechanical-properties-of-slm-fabricated-gh5188-co-superalloy