# Fuzzy and Regression Modeling for Nd: YAG Laser Cutting of Ti-6Al-4V Superalloy Sheet

> Research article (Journal for Manufacturing Science and Production, 2016) · cited 12× · AI/ML

**Wikidata**: [openalex:W2471890212](https://www.wikidata.org/wiki/openalex:W2471890212)  
**Source**: https://4ort.xyz/entity/fuzzy-and-regression-modeling-for-nd-yag-laser-cutting-of-ti-6al-4v-superalloy-sheet