# Elastic Properties of Novel Co- and CoNi-Based Superalloys Determined through Bayesian Inference and Resonant Ultrasound Spectroscopy

> Research article (Metallurgical and Materials Transactions A, 2018) · cited 21× · AI/ML

**Wikidata**: [openalex:W2778737182](https://www.wikidata.org/wiki/openalex:W2778737182)  
**Source**: https://4ort.xyz/entity/elastic-properties-of-novel-co-and-coni-based-superalloys-determined-through-bayesian-inference-and-resonant-ultrasound-