# Elastic-plastic properties of ceramic matrix composites characterization by nanoindentation testing coupled with computer modeling

> Research article (Ceramics International, 2024) · cited 13× · AI/ML

**Wikidata**: [openalex:W4392343408](https://www.wikidata.org/wiki/openalex:W4392343408)  