# Determination of material properties of bulk metallic glass using nanoindentation and artificial neural network

> Research article (Intermetallics, 2022) · cited 25× · AI/ML

**Wikidata**: [openalex:W4213050095](https://www.wikidata.org/wiki/openalex:W4213050095)  
**Source**: https://4ort.xyz/entity/determination-of-material-properties-of-bulk-metallic-glass-using-nanoindentation-and-artificial-neural-network