# Characterization of Ni-Based Superalloy Built by Selective Laser Melting and Electron Beam Melting

> Research article (Metallurgical and Materials Transactions A, 2018) · cited 53× · AI/ML

**Wikidata**: [openalex:W2851976635](https://www.wikidata.org/wiki/openalex:W2851976635)  
**Source**: https://4ort.xyz/entity/characterization-of-ni-based-superalloy-built-by-selective-laser-melting-and-electron-beam-melting