# Automated Method for Fractographic Analysis of Shape and Size of Dimples on Fracture Surface of High-Strength Titanium Alloys

> Research article (Metals, 2018) · cited 43× · AI/ML

**Wikidata**: [openalex:W2791861865](https://www.wikidata.org/wiki/openalex:W2791861865)  
**Source**: https://4ort.xyz/entity/automated-method-for-fractographic-analysis-of-shape-and-size-of-dimples-on-fracture-surface-of-high-strength-titanium-a