# Analysis of intergranular stress corrosion crack paths in gas pipeline steels; straight or inclined?

> Research article (Engineering Failure Analysis, 2017) · cited 16× · AI/ML

**Wikidata**: [openalex:W2771380564](https://www.wikidata.org/wiki/openalex:W2771380564)  
**Source**: https://4ort.xyz/entity/analysis-of-intergranular-stress-corrosion-crack-paths-in-gas-pipeline-steels-straight-or-inclined